View Single Post
  #4 (permalink)  
Old 03-30-2004, 06:40 AM
lloyd lloyd is offline
Newbie
 
Join Date: Jun 2003
Location: BUCKEYE,AZ
Posts: 16
lloyd
Default

MrDmB. I haven't been able to get into the support either. I buff the parts with a spiral sewn wheel with white compound, and it polished up beautifully. The solution doesen't have to be replaced. Your annodes will eventually need to be replaced. I talked to a tech on the phone this morning and he said to try more agitation, but it didn't help so I guess I will have to put up with the gray film and buff it off.
Reply With Quote