CopyCad plating on 62 sq. in. object
I\'m trying to plate motorcycle hubs and sprockets with the CopyCad kit. I\'m getting a rough dull gray plate. I tried a 700ma, 1.5 volt supply with no change in results. I am not sure if I should be increasing voltage or amps to get desired results. Small items such as nuts and bolt plate fine.
Thanks,
Dave
|