I purchased the cheap ($5.00) polishing kit (2 bars, 2 drill wheels) from harborfrieght and it comes with a white and red. My belief is white then red but I still see scratches (very fine ones in the sunshine) in my aluminum pieces. I've been hitting pieces on my VTX but I'm not sure I want to continue until I get these "swirl" scratches resolved. I have also wet sanded these pieces from 320 to 1000. Whats up?