Hello, I tried Copy Chrome 8oz complete set-up today, for the first time, on a fishing reel handle about 3"x 1/2"x 1/8", with a brass base. I compounded the hell out of it, by hand, with automotive polishing compound to remove corrosion on the chrome. It left a somewhat pitted finish with brass base spotting. I buffed any haze off completely with a clean cotton cloth before setting up Copy Chrome. I strted to use Copy Chrome as per instructions. At first it seemed to work, then it started to become a dark & dull, almost nickel looking haze. I rinsed the part afterwards in water to remove any solution. Next, I tried to polish up the new chrome finish with polishing compound to eliminate the darkened haze and all Copy Chrome came off with the dark haze, back to where I started. This is a practice part and after all that, I do need any and all advice. Did I polish part adequitly before plating? Did I move the wand over the part too slowly to create the dark haze? I have antique reels with brass or copper bases and would like to refinish some parts.