Quote:
caswell wrote:
It should all be virtually the same.
Semi-related note: Some people try to use sulfuric acid instead of battery acid....it\'s not the same concentration and doesn\'t work out of the bottle.
|
Hello,
Hope you don\'t mind if I add on to this thread, but what you said caught my eye about sulfuric acid not working out of the box. Can you give a little more detail on that. Reason being we currently use battery acid but my partner seems to think we should switch to sulfuric acid. I did some research and I\'m not sure if I want to use that stuff. If can tell me what the pro\'s and con\'s are that would be great.