You can try stepping back to the brown and buff perpendicular to the scratch lines, then back to the white, perpendicular to the direction you just did the brown in.

I've heard some folks say some talcum powder on a damp wheel will remove fine scratches, but I've never tried it so I can't say if it'd work or not.

Sounds like you're on the right track. With more practice, I'm sure you'll get some really good results.