but i didnt' mention that my buffer is only 2.1 amps. thats very little, i thikn i need a stronger one. w/ that 6 inch wheel, mine bogs down. so i dont know what to do. is that why my parts are not shining up so nicely? it's hard to make ti like perfect.
if someone could give me a list of everythign i should get, i was thinking:
buffer - 6-8 amp
spiril wheel (w/ black compond)
cotton sewn(w/ brown compound) what i currently have
loose cotton (w/ white compound)
white compound
brown compound
black compound
will this produce the results i'm lookign for?
|