Well here is my steps and my 1st PC Part!!! It is a air cooling tube for a V6 Fiero. I think it came out real nice for my first try. I did manage to discover that PC will not fill in scratches very well

I also did not notice any Outgassing at all! I used Gloss Black Powder. Well Here are the Pic's
Here is the tube sanded and cleaned ready to be blasted. I found out playground sand works real well for cleaning but sucks for stripping!

My Infamous Folding Blast cabinet ready to go!

The part after the blast cabinet in the booth waiting on my sorry butt to get set up!

And My Folding Spray Booth ready for action!

Man, parts look fuzzy after getting coated!

Or is that just my crappy camera

??
Here it is in my NON-FOLDING oven just before being removed.

And here it is cooling. I love it, it came out 10000x better than when I started and it was real simple! plus did not tak a whole lot of time, well It took me a long time as I am still learning

And I also made a Folding PArts Arm to hold the parts!