I just replaced my play sand with Aluminum Oxide!( Ihear the sigh's of relief ) and will be testing it tomorrow to see if it works. I am doing some Cadillac 4.9l Valve covers which are Mag. Aircraft stripper worked well but for some reason will not get the factor grey primer off! Will let you know how well this works.