Default Re: problems with bubbles

This problem is addressed in the manual and can be solved by aerating the part with larger bubbles from an airstone during plating.

Please use our technical support section at http://www.caswellplating.com/support.htm to post further technical support related issues. This forum is not set up to handle requests properly and in a timely fashion.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote