View Single Post
  #6 (permalink)  
Old 04-16-2004, 03:05 PM
TCalYen TCalYen is offline
Newbie
 
Join Date: Apr 2004
Location: Ft. Lauderdale, FL
Posts: 12
TCalYen
Default

Quote:
Originally Posted by customandsound
you don't want to use a rotary tool it will take to much time and way to many buff's ..... a goog bench grinder converted will work fine
OK... you're saying that the dremel with not be as effective as a bench grinder with modified fittings to get into the nooks and crannies right? Where can I get some fittings that will get into the nooks and crannies and/or how can I fabricate some

Thanks,
TCalYen
Reply With Quote