powder is only explosive when its in a mist form like when you are spraying it. I had an arc while spraying because I was too close. Only damage was i think my heart skipped a beat when it happened. but the part was fine, had to recoat an area because some of the powder blew off. But I put a part in a gas oven and it cure just fine. But I have an account with a custom bike builder, I use IR propane heat that I got off of ebay for $38. hook it to a propane tank and Im off, Getting a stand with a heater soon to do a guys car. Yeah that whole outside of the car! lol