Default Al welding rod

Neo

Saw this tread a little late but wanted to post to it. We've been using welding rod exclusively for racking and attaching it to an aluminum busbar. A lot of the parts we do suspend very nicely on the J bend or a U bend.
I also use it to connect to my cathodes( 6"x12"plates of 6061..3/8" thick). It tends to get brittle in the anodizing bath but since its disposed of any way its no problem