They\'re 300Watt heaters. You can source them locally at an aquarium dealer.

We don\'t sell converters.

We also won\'t be able to send you the Triple Chrome kit to Hong Kong. It\'s classified as Dangerous Goods for transportation. We can ship this product to California, then you could arrange your own shipping to Hong Kong.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm