it all depends on if it is recomended to clear or not.even if it doesnt it still doesnt hurt to clear it. As for the cure cylce it depends on what your part your doing really. i like to cure mine with the lowest recomended cure cycle, generally just to make sure i dont damage any parts. Really it is just preference on which way you want to go with it. You couls actually cure lower temp but you just have to had time to the cure cycle.