Thanks a TON 48, for your posted procedure (25 NOV '03) this was like a GODSEND as I've been fighting with this 60 year old bathroom faucet ****.......(I mean stuff) for weeks.

YOU DA MAN!

I am still unclear on your definition of "robbers" however, or the particular application you describe. The manual I have, (version 4) describes a "robber" as a way to reduce current, or rather "spread" the current out to ultimately reduce delivery to the work piece.

I do remember reading somewhere how to reduce edge build up by "pig-tailing" wires out from the edges, but I can't remember enough about it to do me any good, or even where I saw it.

Could you please explain how this is done?