MD is correct in that last item.. The wire tends to get brittle as the process progresses. I like to use the "spring"in as deep a hole as possible to assure maximum contact area. Fortunately the parts I'm anodizing have nice deep holes with the exception of one..Not surprisingly thats the one I have the most (but still very few) problems with.
|