Spring tension is exactly what I'm looking for; to hold tiny parts with no holes.

Should we not be concerned with other metals in the alloy contaminating the anodize tank?

Some alloys of titanium even have aluminum in them; would these partially anodize and have to be striped later?

What effect, if any, would deox/desmut have on titanium?