View Single Post
  #8 (permalink)  
Old 05-18-2004, 01:01 PM
ecollins ecollins is offline
Newbie
 
Join Date: Apr 2004
Posts: 8
ecollins
Default better, but not mirror like i see on the web site

First off, the piece has small casting pits that can't be sanded out, without really deforming the shape of the piece. I tried w/an orbital sander and 100 grit sandpaper. They are pretty deep. I think that might be the main problem. Anyway, I'll live with the pits and I just sanded over them. It looks pretty good after the white and loose cotton combo. But then I go to the rouge and canton flannel combo and I still can't get rid of the swirl marks. I wish I had digital camera to post.
-ethan