As long as the parts you want to do will fit in the supplied buckets you can do them with the kit as recieved, with the appropriate sized power source. If the bucket that would be used for the anodizing tank is too small then you can upgrade to a larger container just for that. Like I mentioned previously, the anodizing tank can't be stuffed, so something like a 10-15 gallon anodizing tank is really a pretty good match for 5-6 gallon containers for use in the other processes such as cleaning, dying, sealing and rinsing.