the plating results are the same, i started out brush plating myself but soon learned that tank plating is so much easier and less time consuming, i only use brush plating now for minor touch up work but still use fastgold to do all my gold plating. so yes brushplating would be a good starting point for you. if you are going to use regular chrome you will have to use nickel first.
bill
|