Im switching back because I was getting much better results using the old method. I have since switched to LCD only to get consistently worse results. I truely dont think its building as thick of a layer for me. I know my dyes get no where as deep as they did before. Its simply disturbing seeing my previous results I got when I first set up a small line to try it out as compared to now when I have better equipment and alot more knowledge under my belt.

Basically, im switching back to verify if its me or the something funky going on with the LCD method. If I still get terrible results, ill be back begging for more help from you..........thanks for all the help thus far.