I just tried 1:1(battery acid/water) ratio at 12ASF at 45 minutes for a couple batches, and didnt get the best results. Im going to take your advise Fibergeek, and change the ano bath to 1:2(battery acid/water) to try. Would 12ASF be the best, or do you recommend another current? What time frame do think I should let that in for? Thanks alot!!
|