could lack of cathode area also give results like a described?

I noticed that the cathode that I directly connect my PS lead to puts off alot more bubbles then the rest. I had the others connected together with some fairly decent test leads.....I think the wire thickness may mostly be insulator now that I look closer at them. I ran some 12gauge Al wire to all the plates and not all the plates seem to be putting off about the same bubbles.

If the cathode plates were only "working" very little before, how would that have effected everything?