Quote:
|
Originally Posted by Fibergeek
Hey guys, we put together quite a thread here today.
|
Well, I seem to be making headway over here. So, you dont think there would be a difference from using one 8X8 cathode to using 4 of them since im using CC anodizing? Keep in mind im doing about 150sq. in. batches at this time.
Also, I would love more info on your chiller setup if you wouldnt mind. I like the circulation pump idea, other then the fact that I could picture a hose breaking somewhere and shooting acid all over my workshop. I remember some people having problems with the pumps burning up in the sulfuric acid and grease from the pump making its way into the ano bath. I would consider a system like yours, if it doesnt break the bank TOO bad