You'd really need to submerse the entire part for an even finish.

If they'ew pot metal, you'd need to pot metal prime them, copper plate, nickel plate, chrome plate. Look at our <a href="/triple.htm">Triple Chrome Plating Kit</a>.

It would be extremely difficult to plate these while still attached to the car.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote