Anyone else had the problem of the IR Thermometer not reading right for certain purposes? Was doing a small piece of aluminum that I had glass bead blasted then done in a mirror silver and it kept only saying the piece was about 150 to 180 degrees farheniet. The waves had to be bouncing off of it and on something else partly. Had the piece in a toaster oven set at 400 then I even put it in front of my Mr Heater which was over 1000 degrees and the piece didn't change in temperature. Is there any way to tell if a piece didn't get fully cured? Looks fine to me though...