What is the best way to mask threads and holes?
View Single Post
#
2
(
permalink
)
06-03-2004, 09:56 PM
bhhodges
Moderator
Join Date: Feb 2003
Location: southeast
Posts: 199
any type plastic plugs will work well there is also tape specific for plating you can use to cover threads. i believe caswell sells a kit with various sizes of plugs.