bud you dont want to use the broil setting except for maybe pre-heating the oven....your constant heat will come ffrom the main element, toaster ovens are nasty in that they are far ffrom acurate in the temp guess range ( the dial), youll just have to keep bumping the temp till you get where you want to be, I went down and bought an oven thermstat at coast to coast..couple bucks..anyways it goess to 600f so...with it in the toaster you will at least get a better idea at what your gauge is at, i use a toaster but usually for nuts and bolts ...try finding a used kitchen range if you can..