Some ovens use nichrome wires as elements, usually requires alot of them.The power you would need would kill a battery charger. So to answer you r question- Yes you can make a nichrome heat lamp or oven, I really don't see it as realistic when useing a battery or charger. You would be further ahead to get a LP IR lamp or electric. I always prefer ovens to lamps.