Re: carbon steel sword
Is there any fine detail in this sword that may be lost if polished?
If not, a Spiral Sewn wheel and white buffing compound should make quick work of re-polishing.
I haven\'t tried this on carbon steel, but Coca-Cola does a pretty good job if you just want to dissolve the rust.
|