Yo Bob........
You used to have to go buy an aquarium pump, but now the include a submersible filter/pump because it just works so much better.
The bandages help to keep this really nasty black oxide gunk that forms on the anodes from flying around in your solution, getting all over your parts etc. Wrap them around your anodes with rubber bands.
Have fun.
Dave
|