View Single Post
  #1 (permalink)  
Old 06-16-2004, 01:41 PM
BlindUmpire BlindUmpire is offline
Newbie
 
Join Date: Feb 2004
Posts: 32
BlindUmpire
Default Powder Coating a whole car?

Here's my idea: I want to disassemble my 1969 Bronco and powder coat the hood, fenders, windshield frame, doors and tailgate now that my oven is large enough to handle these parts. The problem is that there are still a few parts that cannot be removed from the truck like both rear quarter panels. I don't have the money for one of the nice IR lamps yet and need ideas on how to cure the powder on these 2 panels. Any ideas? Would a heat gun work well enough for this? Seems like it would produce an uneven cure on such a large panel. I'm open to any ideas. I don't want to bring the tub to a shop and pay someone else to use their oven because I want to leave the tub on the frame with all wiring, etc. intact. Anyone done this before?