Thread
:
Powdercoating black alloy bolts
View Single Post
#
2
(
permalink
)
06-20-2004, 10:15 PM
DALE
Experienced Metal Finisher
Join Date: Dec 2002
Location: Central New York
Posts: 353
The coating is black oxide. If you remove the oils you shouldn't have any problems powdering over that.
DALE
View Public Profile
Send a private message to DALE
Find all posts by DALE