the nickel plating should be a permenant bond so if you are seeing flaking or peeling the only 2 things i can come up with are either surface prep or plating with too many amps. i havent tried to heat anything i have plated but since you brought it up im gonna place something in an oven to around 500 degress just to see what happens----