Default Noob ? about cure temps

Im a noob to PCing. I have two questions. 1st. when a powder says 400 degrees cure time does that mean the metal temp has to be 400 degrees or I set the oven at 400 degrees? 2nd. when I hang a piece up in the oven to bake it do i have to turn it every so often or do i just let it hang the way it is?