Default Filling pits in aluminum casting?

I have had some handles cast, and grind/sand/polish them out. Most however have some air bubble pinholes/pits that are too deep to grind down. I tried Solder-it, but later realized that the casts were aluminum and the solder would not adhere to that. Is there and equivelant aluminum solder type product that would work? I vaguely remember such a low melting point aluminum repair metal (sticks?) I found on the web, but can\'t find it now. Any ideas?

Thanks,

John Henry