A few newbe questions
I received a copy chrome kit and have a few questions before the actual start.
1-In two different spots in the manual it says two different solution make-ups of the SP Degreaser. Is it 8oz to 1 gal of water or 12 oz to 3 gal of water?
2-Do I have to have copper flash for alum. and steel?
3-The Zincate solution is fuzzy to me.Does it mean 25% solution to 1 full water,ie..1 gal of water to 1/4 gal solution?
4-And finally when mixing the copy chrome solution,during the 24 hr stew/dissolve period does it need to be heated all that time?
Thank you in advance for the help and I hope that these are not I,D,10,T questions.