I opened a bottle of 24K gold plating solution I purchased about a year ago. I noticed that the gold had deposited on the wall of the plastic bottle.
After shaking up, most of the gold came off the bottle and settled to bottom. I now have a light green liquid with what looks like flakes of gold leaf on bottom. Is there a way to put the gold back into solution or should I write it off as a bad buy.
Thanks,
Jerry