I have done a few pieces with it. It's one of those colors that varies quite a bit with dye time. Never had problems using it, just had to dip, rinse and check several times to get the shade wanted.
SS
hey my friend got his ripper one back today and he wants brown and olive. i have brown, but i've heard that olive is hard to get right. does anyone have any input? is caswells olive dye good? if anyone can help me out that would be very appreciated. thanx!
I have done a few pieces with it. It's one of those colors that varies quite a bit with dye time. Never had problems using it, just had to dip, rinse and check several times to get the shade wanted.
SS
I have a dye of Olive Drab from a company called Clariant.
I personally like it better, however its the same as what SS said, it varies a lot since its a shading colour, you have to keep an eye on it.
ok thanx guys.