Default How much to anodize?

I was thinking of getting some aluminum wheels anodized black, but I have no idea how much something like this would cost. I did a search on here, but didn't find anything. Anyone have any idea how much I could expect to pay? Just an idea really. It will be 4 brand new aluminum wheels for an ATV (two 9x9 and two 10x5). The few local places I called wouldn't do a "small" job like this. Thanks
Reply With Quote
  #2 (permalink)  
Old 02-02-2004, 03:41 PM
Amateur Metal Finisher
 
Join Date: Mar 2003
Posts: 162
NeoMoses
Send a message via AIM to NeoMoses Send a message via Yahoo to NeoMoses
Default

The last time I quoted anodizing, I was looking at a minimum cost of around $300 per batch. A friend of mine has his parts anodized by M.A.X. anodizing in Texas. They do exceptional work and are not terribly expensive. http://www.maxanodizing.com/index2.html

Are the wheels currently anodized? If not, they might not be a good alloy for anodizing, anyway. You might look into powder coating them as well. It could be cheaper and still look very nice.
Reply With Quote
  #3 (permalink)  
Old 02-02-2004, 06:47 PM
M_D M_D is offline
Amateur Metal Finisher
 
Join Date: Dec 2003
Posts: 219
M_D
Default

The commercial anodizer we use has a minimum of $75 per color, per order, I'm fairly sure that your wheels would cost no more than that from them.
Reply With Quote
  #4 (permalink)  
Old 02-02-2004, 09:20 PM
Newbie
 
Join Date: Jan 2004
Posts: 3
fade2black
Default

I finally found a local place that would do the job for me. I couldn't believe the price....$10 per wheel! The guy said they do them all the time. Thanks for the answers.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
LCD anodize of a large piece? scocklin Anodizing Questions 2 12-29-2004 12:21 AM
Combined powder coat & anodize seanc Powder Coating Questions 3 09-03-2004 12:31 PM
A question for the anodize boys from the powder guy non-stick Anodizing Questions 3 11-26-2003 04:22 PM
How do I Hardcoat Anodize (Type III)? 00_buckshot Anodizing Questions 2 09-09-2003 01:10 AM
Basic anodize questions erogers Anodizing Questions 0 03-12-2003 07:54 PM


All times are GMT -4. The time now is 06:35 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.