I'm wondering how solder aluminum will react to anodizing if anyone had done this. What I have is two tubes that I'm putting together at 90* hopefully with aluminum solder which is zinc and aluminum. Will this have a big problem dissolving during the process?
|
|
|||
|
Its difficult to say, not because of the Aluminum, but because of the Zinc. It probably depends on the % of Zinc in the solder and the amount of solder used. The zinc may dissolve in the electrolyte during the anodizing process, but another concern would be the contamination of the elctrolyte by the zinc, which could ruin the entire anodizing process.
The only way to tell for sure is to try to anodize just a small piece of the solder and see it the concentration of Zinc in it causes any problems. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Something for you die hard polishers out there to chew on | thesound | Metal Polishing Questions | 15 | 12-03-2007 01:16 PM |
| Prepping/polishing aluminum for 'brite dip' anodizing | mark369 | Metal Polishing Questions | 0 | 02-05-2005 02:00 AM |
| stripping anodizing off aluminum | broker1234 | Metal Polishing Questions | 1 | 01-16-2005 10:28 PM |
| Anodizing 7000 series aluminum | oneartisan | Anodizing Questions | 1 | 05-11-2003 01:55 PM |
| Aluminum Solder Paste | trw | Other Metal Finishing Questions | 2 | 03-25-2003 09:55 AM |