Default Phosphori Acid Anodization

I am a student trying to anodize some AL 6061-T6 for research. My intentions are to do a FPL pretreatment and then Phosphoric Acid Anodization.
I am reading from text that the FPL etch bath needs a compistion of 15.0 parts FeS0(4) 37 parts H(2)SO(4) and 48 parts H(2)O and the PAA to have 100 g/L H(3)PO(4).

I am interested in the following questions:

1. Is FPL and PAA safe enough to do in a lab (fume hood is accesible)?
2. If 1. is yes, is there a kit with specified solutions above?
3. If no kit is available with those solutions, can I buy a kit and then use my own solutions obtained elsewhere?

I appreciate all the help...thank you.
Reply With Quote
  #2 (permalink)  
Old 06-15-2005, 11:49 PM
sswee's Avatar
Moderator
 
Join Date: Nov 2004
Location: close to Austin, Texas
Posts: 1,230
sswee is a jewel in the roughsswee is a jewel in the roughsswee is a jewel in the roughsswee is a jewel in the rough
Default

Not knowing the procedures for PAA, can't say what would work. This forum deals with LCD anodizing. Type II sulfuric. Sorry, can't be of help.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Acid SniperSlayer Anodizing Questions 8 07-25-2005 10:59 PM
Acid copper Gabourie Electroplating Questions 3 09-25-2004 09:42 PM
"Sandwiching" Acid Copper AresP Electroplating Questions 1 08-27-2004 09:19 PM
Acid concentration versus current density M_D Anodizing Questions 7 02-04-2004 10:01 PM
Acid Bath Content? Chevalier Anodizing Questions 3 01-12-2004 11:46 PM


All times are GMT -4. The time now is 04:42 AM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.