I use the NAPA auto parts 5 gallon containers for anodizing and I mix 3:1 ratio with awsome results,





Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Acid SniperSlayer Anodizing Questions 8 07-25-2005 10:59 PM
Acid copper Gabourie Electroplating Questions 3 09-25-2004 09:42 PM
"Sandwiching" Acid Copper AresP Electroplating Questions 1 08-27-2004 09:19 PM
Acid concentration versus current density M_D Anodizing Questions 7 02-04-2004 10:01 PM
Acid Bath Content? Chevalier Anodizing Questions 3 01-12-2004 11:46 PM


All times are GMT -4. The time now is 05:13 AM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.