Default Very easy to do!!

I have wanted to try anodizing for a long time. I mainly wanted to to model airplane engine parts. I got everything set up this past weekend and using items from Caswell was able to get parts anodized and colored the first try through! If you are someone wanting to try do it, it really is very easy to do!

Tim Wiltse
Reply With Quote
  #2 (permalink)  
Old 10-07-2002, 08:27 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,356
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default Your Comments

Thanks for the nice comments.

Is it OK if we add your comments to our testimonials section at http://www.caswellplating.com/testimonials.htm?
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
OnLine Easy Answers - Surface Area Calculator charlton Electroplating Questions 3 07-31-2005 06:01 PM
quick and easy degreasing customandsound Electroplating Questions 6 07-29-2005 03:50 PM
Calculating Surface Area, the Easy Way. PrecisionPB Anodizing Questions 6 05-28-2005 02:56 PM
easy pic posting non-stick Powder Coating Questions 2 12-08-2003 02:06 PM
Is it this easy, or am I missing something? golferdude Powder Coating Questions 18 07-12-2003 12:21 AM


All times are GMT -4. The time now is 01:53 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.