They're the same thing.
The aluminum de-oxidizer product we sell at http://www.caswellplating.com/aluminum.htm is a de-smutting agent.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| De smut | TamRon | Electroplating Questions | 3 | 03-09-2005 12:14 AM |
| Smut? | scocklin | Anodizing Questions | 3 | 12-01-2004 09:13 PM |
| finishing techniques | sgunn911 | Anodizing Questions | 10 | 06-20-2004 02:39 PM |
| what do I do with all this smut!!! | krsimulis | Anodizing Questions | 2 | 06-05-2004 08:23 PM |
| stripping smut | johnlindahl | Electroplating Questions | 1 | 11-01-2002 08:57 AM |