+ Reply to Thread
Page 3 of 3
FirstFirst 1 2 3
Results 21 to 23 of 23

Thread: Help!!!

  1. #21

    Default Re: Help!!!

    Hey everyone sorry about the long silence, life you know sometimes takes over!
    In any case, tried my new dyes and set up out, the first run my wire anodized, but not the part, I already know why( I've been reading). the next patch came out great!!! I did this little airbrush stand for my buddy, and it came out a nice deep red!!! I could NOT be happier!!!
    SS, I will be getting a PS soon, I hope.
    I also will be starting to "play" around with masking and try a fade, this is great THANKS everyone!
    Canute
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  2. #22
    Join Date
    Nov 2004
    Location
    close to Austin, Texas
    Posts
    1,283

    Default Re: Help!!!

    Good to hear. A few good results make the troubles and hassles seem not so bad. Post some pics if you can.
    SS
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  3. #23

    Default Re: Help!!!

    SS, I ordered my power supply yesterday, should be here next week. I got a digital CC/CV 3amp unit, it should easily handle the size of operation that I currently have.
    Sorry can't do pix at this time, I'm not up to date on all the gizmos (my computer still is using windows9, I may be able to come up w/ pix later on.
    Thanks again,
    Canute
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

+ Reply to Thread
Page 3 of 3
FirstFirst 1 2 3

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

     

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts

Search Engine Friendly URLs by vBSEO 3.5.0 RC1 PL1