Default Should I order more Ti?

I've been PM'd by a couple of you about getting more titanium wire for racking. I'm down to just a couple 3' pieces of 1/16in.
If you guys want more of both 1/16in, and 1/8in, chime in here with how much you might need. The 1/16in comes in 3' lengths, and I have to buy 40 pieces for $80 (minimum order). The 1/8in comes in up to 8' lengths, and can be purchaced individually.
Prices will be same as last time (I only charge what it costs me)...
1/16in up to 3' lengths- $.66 per foot.
1/8in up to 8' lengths- $3 per foot.
Prices do not include shipping.
__________________
Specializing in anodized graphics in Paintball guns.
Reply With Quote
  #2 (permalink)  
Old 07-13-2006, 08:27 PM
destroyer125's Avatar
Experienced Metal Finisher
 
Join Date: Jul 2005
Posts: 443
destroyer125 is an unknown quantity at this point
Default Re: Should I order more Ti?

I would like some
Reply With Quote
  #3 (permalink)  
Old 07-14-2006, 08:13 PM
Amateur Metal Finisher
 
Join Date: Aug 2005
Posts: 116
rclint is an unknown quantity at this point
Default Re: Should I order more Ti?

Sending a pm as well

Can you get TI machine type screws ? I have a guy I anodize parts for, small parts with zero blemish on outside, 8-32 threads if I remember correctly. 20 would be perfect, but I don't make much money at all of these, so not wanting to sink in 3 or 4 runs of these parts to pay for them LOL

Clint
Reply With Quote
  #4 (permalink)  
Old 07-14-2006, 08:24 PM
Amateur Metal Finisher
 
Join Date: Aug 2005
Posts: 116
rclint is an unknown quantity at this point
Default Re: Should I order more Ti?

acidrain

Please clear your pm box, trie to send you a pm, it's full

Thanks, Clint
Reply With Quote
  #5 (permalink)  
Old 07-14-2006, 10:49 PM
Metal Finishing Guru
 
Join Date: Sep 2004
Posts: 829
acidrain is on a distinguished road
Default Re: Should I order more Ti?

OK, box is empty now.
I have lots 10-32 screws, but no 8's.
I can let the nuts or screws go for $.50 ea. (have you guys priced this stuff?).
I won't be able to get the 1/16in, unless we can get more guys on-board. I suppose I could run the left-overs on e-bay, but I really don't want to have to do that.
I think it was Yoyoboy that wanted some. You out there?
Maybe I'll post on PBnation too.
__________________
Specializing in anodized graphics in Paintball guns.
Reply With Quote
  #6 (permalink)  
Old 07-14-2006, 11:52 PM
Amateur Metal Finisher
 
Join Date: Aug 2005
Posts: 116
rclint is an unknown quantity at this point
Default Re: Should I order more Ti?

I have priced it... and purchased some, I have a lot of Ti wire myself , I need to move half or more of it, forget the exact stuff I have tho LOL. I also noted when I used the wire (anodized with it) it turned a very dark color, black/purple, and swore it took die lol, I guess the dye just clung to the wire, because it washed off. The Ti is nice when you have alot of the same parts, not trie dthe screws yet, justa good snug threading that bottoms out will work good ?


Clint
Reply With Quote
  #7 (permalink)  
Old 07-15-2006, 12:16 AM
Metal Finishing Guru
 
Join Date: Sep 2004
Posts: 829
acidrain is on a distinguished road
Default Re: Should I order more Ti?

I have about four pieces of the 1/8in that I have threaded about 1/4in of the ends with 6-32 threads. The die cuts a cone shape where the threads begin on the rod. When threading this racking wire into a part, it snugs up against the cone shape.
The Ti is very easy to thread... just like steel.
I have one piece of 1/4in rod that I narrowed the end on (with a belt sander), and then threaded with 10-32. Threading your racking rod/wires is a very good way to go. Just keep in mind this is where acid will hide when you go to dye your parts.
__________________
Specializing in anodized graphics in Paintball guns.
Reply With Quote
  #8 (permalink)  
Old 07-20-2006, 03:46 PM
Metal Finishing Guru
 
Join Date: Sep 2004
Posts: 829
acidrain is on a distinguished road
Default Re: Should I order more Ti?

My Ti guy is out, and the stuff is on back order. Anybody wanting to get in on an order needs to post here exactly how much of each size they need, then I'll PM you with how to pre-pay.
__________________
Specializing in anodized graphics in Paintball guns.
Reply With Quote
  #9 (permalink)  
Old 07-20-2006, 11:05 PM
ken_the_stp's Avatar
Newbie
 
Join Date: Jun 2006
Location: Evans Mills NY
Posts: 33
ken_the_stp is on a distinguished road
Send a message via AIM to ken_the_stp Send a message via Yahoo to ken_the_stp
Default Re: Should I order more Ti?

I am posting here just as a curtsy since I had asked you in an email about the TI.

I just won 185 feet of some 1/32" type 2 off ebay. So I will not go in on the TI this time around.
Reply With Quote
  #10 (permalink)  
Old 07-20-2006, 11:15 PM
Metal Finishing Guru
 
Join Date: Sep 2004
Posts: 829
acidrain is on a distinguished road
Default Re: Should I order more Ti?

Oh wow... good one! Maybe you'll want to share with us?
__________________
Specializing in anodized graphics in Paintball guns.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
order of polishing honda900 Metal Polishing Questions 1 08-07-2003 12:43 PM
Order mr.wagon Services Offered/Wanted 5 08-06-2002 07:04 PM


All times are GMT -4. The time now is 05:49 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.