I was wondering if anyone had any different problems using different colors of RIT dye to color your anodized part?
I did a part the other night and used the Royal blue color on it and it turned out just fine, although it was a little more purple than I wanted. But I did some parts last night, the exact same way I did the first ones but I used the dark green dye this time, and when I sealed the part almost all of it came off leaving a real light green when I wanted a dark green. Are there differences in the colors that one will work better than the others? I just ordered some dyes from Caswell today in hopes that will fix my problem. Anyone know if the Caswell green is a real bright one? |
|
||||
|
Answered in other forum.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Color depth vs. anodizing time | NeoMoses | Anodizing Questions | 17 | 02-03-2004 09:06 PM |
| Anodizing different alloys | TONYZ | Anodizing Questions | 2 | 11-02-2003 01:31 PM |
| opaque anodizing dyes | july_favre | Anodizing Questions | 1 | 03-12-2003 08:26 PM |
| Anodizing using RIT dyes Question | Hcues1 | Other Metal Finishing Questions | 3 | 03-03-2003 08:35 PM |
| dumb anodizing question | felix | Electroplating Questions | 1 | 08-06-2002 08:37 AM |