Default Acid wash

Do any of you have any info on how to do acid wash? I don't know much about it other then it looks cool on paintball guns.

Thanks.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
acid wash examples -AAPB-Eric Anodizing Questions 3 05-20-2006 08:31 PM
Acid Wash for header prior to Ceramic Coating Timmer Powder Coating Questions 9 05-09-2006 01:27 PM
Acid SniperSlayer Anodizing Questions 8 07-25-2005 09:59 PM
Acid concentration versus current density M_D Anodizing Questions 7 02-04-2004 09:01 PM


All times are GMT -4. The time now is 08:14 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.